Sign In | Join Free | My chinacomputerparts.com
China ZEIT Group logo
ZEIT Group
Pursuing Excellence without Limits!
Active Member

5 Years

Home > Atomic Layer Deposition Equipment >

Protective Coating Field Atomic Layer Deposition System Seal Coating

ZEIT Group
Contact Now

Protective Coating Field Atomic Layer Deposition System Seal Coating

Brand Name : ZEIT

Model Number : ALD-PC-X—X

Certification : Case by case

Place of Origin : Chengdu, P.R.CHINA

MOQ : 1set

Price : Case by case

Payment Terms : T/T

Supply Ability : Case by case

Delivery Time : Case by case

Packaging Details : Wooden case

Weight : Customizable

Size : Customizable

Guarantee period : 1 year or case by case

Customizable : Available

Shipping Terms : By Sea / Air / Multimodal Transport

Contact Now

Atomic Layer Deposition in Protective Coating Field


Applications

Applications Specific Purpose
Protective coating

Corrosion-resistant coating

Seal coating


Working Principle
In a traditional CVD process, the gas-phase precursors will continuously or at least partially react. In the ALD
process, however, the reactions only occur on the substrate surface. It is a cyclic process consisting of multiple
partial reactions, that is, the substrate contacts with precursors in sequence and reacts asynchronously. At any
given time, only parts of the reactions occur on the substrate surface. These different reaction steps are self-limiting,
that is, the compounds on the surface only can be prepared from precursors suitable for film growth. Partial reactions
are completed when the spontaneous reactions no longer occur. The process chamber will be purged and/or emptied
by inert gas among different reaction steps in order to remove all the pollutants generated by precursor molecules in
the previous processes.

Features

Model ALD-PC-X—X
Coating film system AL2O3, TiO2, ZnO, etc
Coating temperature range Normal temperature to 500℃ (Customizable)
Coating vacuum chamber size

Inner diameter: 1200mm, Height: 500mm (Customizable)

Vacuum chamber structure According to customer’s requirements
Background vacuum <5×10-7mbar
Coating thickness ≥0.15nm
Thickness control precision ±0.1nm
Coating size 200×200mm² / 400×400mm² / 1200×1200 mm², etc
Film thickness uniformity ≤±0.5%
Precursor and carrier gas

Trimethylaluminum, titanium tetrachloride, diethyl zinc, pure water,
nitrogen, etc.

Note: Customized production available.


Coating Samples
Protective Coating Field Atomic Layer Deposition System Seal CoatingProtective Coating Field Atomic Layer Deposition System Seal Coating
Process Steps
→ Place the substrate for coating into the vacuum chamber;
→ Vacuumize the vacuum chamber at high and low temperature, and rotate the substrate synchronously;
→ Start coating: the substrate is contacted with precursor in sequence and without simultaneous reaction;
→ Purge it with high-purity nitrogen gas after each reaction;
→ Stop rotating the substrate after the film thickness is up to standard and the operation of purging and cooling is

completed, then take out the substrate after the vacuum breaking conditions are met.

Our Advantages
We are manufacturer.
Mature process.
Reply within 24 working hours.

Our ISO Certification
Protective Coating Field Atomic Layer Deposition System Seal Coating


Parts Of Our Patents
Protective Coating Field Atomic Layer Deposition System Seal CoatingProtective Coating Field Atomic Layer Deposition System Seal Coating


Parts Of Our Awards and Qualifications of R&D

Protective Coating Field Atomic Layer Deposition System Seal CoatingProtective Coating Field Atomic Layer Deposition System Seal Coating























































Product Tags:

Protective Coating Field Atomic Layer Deposition

      

Protective Coating Field atomic layer deposition system

      

atomic layer deposition system Seal coating

      
China Protective Coating Field Atomic Layer Deposition System Seal Coating factory

Protective Coating Field Atomic Layer Deposition System Seal Coating Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: ZEIT Group
*Subject:
*Message:
Characters Remaining: (0/3000)